<dc schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/ http://www.openarchives.org/OAI/2.0/oai_dc.xsd"><type>Thesis:Masters</type><title>Sifat korosi dan "creep" ni-base super alloy</title><creator>Renaningsih Setjo A, author</creator><creator>Add author: Parangtopo Sutokusumo, supervisor</creator><creator>Add author: Dewa Nyoman Adnyana, examiner</creator><creator>Add author: Na, Peng Bo, examiner</creator><creator>Add author: Darmadi Kusno, examiner</creator><creator>Add author: Silva, B.E.F. da, examiner</creator><creator>Add author: Suhardjo Poertadji, examiner</creator><publisher/><date>1988</date><subject>Corrosion resistant alloys</subject><description><b>ABSTRAK</b><br>
Telah dilakukan penelitian tentang sifat korosi dari empat macam "Ni base" aloi yaitu Incoloy 800 H, Hastelloy XR, Inconel 617 dan Ni-CR-W pada temperatur 950° C selama 300 jam di dalam lingkungan udara dan helium.
<br><br>
Dari pengamatan yang dilakukan terhadap laju korosi dan ketebalan lapisan film yang terbentuk pada permukaan spesimen, terjadinya korosi dalam butir dan batas butir, ternyata bahwa Hastelloy XR dan aloi Ni-Cr-W mempunyai ketahanan yang cukup tinggi terhadap korosi khususnya dalam lingkungan helium.
temperatur 950° C selama 300 jam di dalam lingkungan udara dan helium.
<br><br>
Percobaan "creep" dilakukan terhadap Hastelloy XR, Incoloy 800 H dan aloi Ni-CR-W, pada temperatur 900°C, dalam udara, dengan variasi tegangan. Diperoleh bahwa Ni-CR-W mempunyai ketahanan yang baik terhadap "Creep" karena presipitasi &#945; -W yang homogen di dalam butir.</description><identifier>http://lontar.ui.ac.id/detail?id=82685</identifier><recordID>82685</recordID></dc>
|
format |
Thesis:Masters Thesis Thesis:Bachelors |
author |
Renaningsih Setjo A, author Add author: Parangtopo Sutokusumo, supervisor Add author: Dewa Nyoman Adnyana, examiner Add author: Na, Peng Bo, examiner Add author: Darmadi Kusno, examiner Add author: Silva, B.E.F. da, examiner Add author: Suhardjo Poertadji, examiner |
title |
Sifat korosi dan "creep" ni-base super alloy |
publishDate |
1988 |
topic |
Corrosion resistant alloys |
url |
http://lontar.ui.ac.id/detail?id=82685 |
contents |
<b>ABSTRAK</b><br>
Telah dilakukan penelitian tentang sifat korosi dari empat macam "Ni base" aloi yaitu Incoloy 800 H, Hastelloy XR, Inconel 617 dan Ni-CR-W pada temperatur 950° C selama 300 jam di dalam lingkungan udara dan helium.
<br><br>
Dari pengamatan yang dilakukan terhadap laju korosi dan ketebalan lapisan film yang terbentuk pada permukaan spesimen, terjadinya korosi dalam butir dan batas butir, ternyata bahwa Hastelloy XR dan aloi Ni-Cr-W mempunyai ketahanan yang cukup tinggi terhadap korosi khususnya dalam lingkungan helium.
temperatur 950° C selama 300 jam di dalam lingkungan udara dan helium.
<br><br>
Percobaan "creep" dilakukan terhadap Hastelloy XR, Incoloy 800 H dan aloi Ni-CR-W, pada temperatur 900°C, dalam udara, dengan variasi tegangan. Diperoleh bahwa Ni-CR-W mempunyai ketahanan yang baik terhadap "Creep" karena presipitasi α -W yang homogen di dalam butir. |
id |
IOS18064.82685 |
institution |
Universitas Indonesia |
institution_id |
51 |
institution_type |
library:university library |
library |
Perpustakaan Universitas Indonesia |
library_id |
492 |
collection |
Repository Skripsi (open) Universitas Indonesia |
repository_id |
18064 |
city |
KOTA DEPOK |
province |
JAWA BARAT |
repoId |
IOS18064 |
first_indexed |
2022-12-13T09:16:49Z |
last_indexed |
2022-12-13T09:16:49Z |
recordtype |
dc |
merged_child_boolean |
1 |
_version_ |
1752208049798381568 |
score |
17.206863 |